High resistivity wafers
1997-07-31
Tony Rogers
High resistivity wafers
Tony Rogers
1997-07-31
I am having difficulty locating a source of FZ wafers with the
following spec.

* Orientation: <100>
* Resistivity: >1000 Ohm cm
* Thickness: 525 microns (or thicker)
* Dia.  100mm preferable
* Quantity:  Initially I need just 12 wafers but will purchase a
larger batch if necessary.

Can anybody supply these or offer any advice on where to obtain
them?




--
Tony Rogers
Applied Microengineering Ltd (AML)
68 Milton Park, Abingdon, OXON, OX14 4RX, UK
Tel: +44 (0) 1235 833 934
Fax: +44 (0) 1235 833 935
WWW: http://www.aml.co.uk


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Nano-Master, Inc.
Harrick Plasma, Inc.
Mentor Graphics Corporation