A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: bio-compatible adhesive material
bio-compatible adhesive material
2003-04-14
Kyutae Yoo
2003-04-14
Jaephil Do
fusion bonding
2003-04-15
Vittorio Guarnieri
bio-compatible adhesive material
Jaephil Do
2003-04-14
We used UV curable adhesive. For the exact patterning, screen printing,
and normal UV aligner can be used.

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Kyutae Yoo
Sent: Sunday, April 13, 2003 8:22 PM
To: [email protected]
Subject: [mems-talk] bio-compatible adhesive material

Hello,

I am looking for a bio-compatible adhesive material(glue) for wafer
bonding.
Does anyone know such material or have used it for wafer bonding?
Thank you

sincerely,
------------------------------------------------
Kyutae Yoo, Ph.D.

MEMS Lab
Samsung Advanced Institute of Technology (SAIT)
Tel(Office)   : +82-31-280-6948
Fax(Office)  : +82-31-280-8277
Tel(Mobile) : +82-11-345-5641

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Addison Engineering