MEMSnet Home: MEMS-Talk: Plasma etching (PR as mask)
Plasma etching (PR as mask)
2003-04-14
Hoyin
2003-04-14
Chan Ho Yin
2003-04-16
Shay Kaplan
Plasma etching (PR as mask)
Chan Ho Yin
2003-04-14
Hi all,

    I have tried to etch a polymer layer by means of plasma etching and
used PR(AZ5214E) as mask. However, I found that the PR is not easily
washed away by acetone after plasma etching. When the PR is dipped under
acetone, it turns into many small pieces and stick on the substrate. Why?
Have you met this problem? is it the power of the RF too large (60W)?  Or
what?  Please help..

Thank you very much!

Best regards,
Hoyin


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
Harrick Plasma, Inc.
MEMS Technology Review