A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: help for silicon etching
help for silicon etching
2003-06-26
Sukanta
2003-06-26
Michaela Wullinger
2003-06-26
[email protected]
2003-06-26
[email protected]
2003-06-26
M.C Liu
2003-06-26
Pavel Neuzil
2003-06-28
Phillipe Tabada
2003-06-30
Echeverria, Jon Ander
help for silicon etching
Sukanta
2003-06-26
Hi
  Can anybody help me how to do chemical etching of silicon.what
chemicals and at what solutions it should be used.
please help

sukanta

Optoelectronics division
SAMEER
IIT powai campus
mumbai-76


sukanta Debbarma
Scientific officer
SAMEER,IIT Mumbai-400076
___________________________________________________
Click below to experience Sooraj Barjatya's latest offering
'Main Prem Ki Diwani Hoon' starring Hrithik Roshan,
Abhishek Bachchan & Kareena Kapoor http://www.mpkdh.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
The Branford Group
MEMS Technology Review