A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: help for silicon etching
help for silicon etching
2003-06-26
Sukanta
2003-06-26
Michaela Wullinger
2003-06-26
[email protected]
2003-06-26
[email protected]
2003-06-26
M.C Liu
2003-06-26
Pavel Neuzil
2003-06-28
Phillipe Tabada
2003-06-30
Echeverria, Jon Ander
help for silicon etching
Phillipe Tabada
2003-06-28
For both KOH and HNA you can use a nitride mask.  For a better etch stop
when removing the nitride people generally place a thin oxide layer
underneath the nitride


Phil Tabada


>From: "M.C Liu" 
>Reply-To: General MEMS discussion 
>To: "General MEMS discussion" 
>Subject: Re: [mems-talk] help for silicon etching
>Date: Fri, 27 Jun 2003 06:48:58 -0000
>
>I had used KOH and HNA in my experiment.But I can't get a satisfied result
>to use nickel mask in KOH and photoresist mask in HNA.Waht's a convenient
>material for mask?
>
>
>----- Original Message -----
>From: 
>To: Sukanta ; General MEMS discussion
>
>Sent: Thursday, June 26, 2003 3:56 PM
>Subject: Re: [mems-talk] help for silicon etching
>
>
> > There are many chemical processes for etching silicon available in the
>literature. Depending on masking material if any that is being used and the
>rate of silicon etch you are looking for we use to use an HF/Acetic/Nitric
>acid. The reaction is very strong with good exhaust required to prevent
>exposure to the operator but is will etch silicon. Bob Henderson
>
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/

_________________________________________________________________
Add photos to your e-mail with MSN 8. Get 2 months FREE*.
http://join.msn.com/?page=features/featuredemail


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing