MEMSnet Home: MEMS-Talk: Aluminum etched by developer
Aluminum etched by developer
2003-08-08
LSWANG
2003-08-09
alfred renaldo
2003-08-11
Jim Beall
2003-08-08
Michael D Martin
2003-08-10
Pavel Neuzil
2003-08-10
[email protected]
2003-08-11
Jobert van Eisden
Aluminum etched by developer
Jim Beall
2003-08-11
You might try Shipey CD-30 developer which has worked for folks here
making thin Al devices.

According to a paper at:
http://marcuslab.harvard.edu/how_to/reliable_liftoff.PDF
this is because it "contains a phosphate, which passivates aluminum."

Jim


>Hi,there,
>Anyone has experience with patterning Al. I got
>problem when developing the photoresist, the Al layer
>is etched by the developer. I tried SHipley and AZ
>resists, but both have the same problem. THanks
>Lisen
>
>__________________________________
>Do you Yahoo!?
>Yahoo! SiteBuilder - Free, easy-to-use web site design software
>http://sitebuilder.yahoo.com
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/


--

  - Jim Beall 303-497-5989
    [email protected]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Tanner EDA by Mentor Graphics
University Wafer
The Branford Group