MEMSnet Home: MEMS-Talk: cleaning small chips
cleaning small chips
2003-12-20
Jen Robertson
2003-12-22
Vonda C Alexander
2003-12-22
Steven F. Nagle
2003-12-23
Absara Micro Systems
YBCO contamination?
2004-01-08
Oray Orkun Cellek
2003-12-25
Jack Mulligan
2003-12-21
Phillipe Tabada
2003-12-21
Phillipe Tabada
2003-12-23
Jason Viotty
2003-12-23
Bill Moffat
cleaning small chips
Phillipe Tabada
2003-12-21
Hi Jen,

  If your mems devices have "no free hanging structures" and are somewhat
physically resiliant, you can try the method described below.  However, for
this method to work you require a custom jig which allow liquid to flow
freely across your dice.

1.  Recirculating PR stripper solution (with filter if possible)
2.  Recirculating acetone
2.  Methanol dip
4.  Recirculating water soak with resistivity monitor
5. Spin cycle

Phil Tabada
UC Davis PhD Candidate

>From: Jen Robertson 
>Reply-To: General MEMS discussion 
>To: [email protected]
>Subject: [mems-talk] cleaning small chips
>Date: Fri, 19 Dec 2003 17:04:59 -0800 (PST)
>
>Hi-
>
>Is there a good way to clean small (<5mm square) silicon chips? Our chips
>have lots of visiable residues after the dicing process, either from the
>dicing tapes or wafer dusts. We have tried soaking in many different
>solvents but cannot seem to get rid of them. These chips have fragile MEMS
>structures on them and will break if we use ultrasonic agitation. Any
>suggestion would be greatly appreciated. Thanks!
>
>
>Jen
>
>
>---------------------------------
>Do you Yahoo!?
>Free Pop-Up Blocker - Get it now
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/

_________________________________________________________________
Have fun customizing MSN Messenger — learn how here!
http://www.msnmessenger-download.com/tracking/reach_customize



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Nano-Master, Inc.
Mentor Graphics Corporation