MEMSnet Home: MEMS-Talk: YBCO contamination?
cleaning small chips
2003-12-20
Jen Robertson
2003-12-22
Vonda C Alexander
2003-12-22
Steven F. Nagle
2003-12-23
Absara Micro Systems
YBCO contamination?
2004-01-08
Oray Orkun Cellek
2003-12-25
Jack Mulligan
2003-12-21
Phillipe Tabada
2003-12-21
Phillipe Tabada
2003-12-23
Jason Viotty
2003-12-23
Bill Moffat
YBCO contamination?
Oray Orkun Cellek
2004-01-08
Dear Mems-Talk Users,

Is YBCO a contaminant material for the III-V and II-VI processing
environement ?  We plan to sputter YBCO in a chamber used for GaAs and
HgCdTe processing.  May any residue of YBCO become harmful to these
materials ?

Thank you  for your  answers,

Best regards,

Oray Orkun Cellek
Research Assistant, Ph. D. Student
Electrical & Electronics Engineering Department
Middle East Technical University
06531 Ankara
Turkey
Tel : +90 312 210 4579
Fax : +90 312 210 1261
e-mail : [email protected]



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
University Wafer