MEMSnet Home: MEMS-Talk: APC angle in ICP process
APC angle in ICP process
2004-01-13
[email protected]
2004-01-13
Tony Li
2004-01-14
[email protected]
2004-01-14
Blunier, Stefan
APC angle in ICP process
[email protected]
2004-01-13
Hi,
Am using an STS ICP Deep Reactive Ion Etcher. Have noticed that the APC angle
is slightly different in different protocols and this seems to affect the etch
outcome. Could I ask what is APC angle and how does it affect etch profile and
speed. Thanks.

Regards,
Melissa



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
The Branford Group
Mentor Graphics Corporation
MEMS Technology Review