MEMSnet Home: MEMS-Talk: APC angle in ICP process
APC angle in ICP process
2004-01-13
[email protected]
2004-01-13
Tony Li
2004-01-14
[email protected]
2004-01-14
Blunier, Stefan
APC angle in ICP process
Blunier, Stefan
2004-01-14
Hi Melissa
Why don“t you ask STS in UK directly?
As far as I understand: The APC angle is the opening angle of the butterfly
valve
between the vacuum chamber and the turbo pump.
It will affect the pressure in the chamber. Comparing the pressures during
etching
while running your different protocols should show it.
Greetings
Stefan

-----Original Message-----
From: [email protected] [mailto:mems-talk-
[email protected]] On Behalf Of [email protected]
Sent: Dienstag, 13. Januar 2004 07:29
To: General MEMS discussion
Subject: [mems-talk] APC angle in ICP process



Hi,
Am using an STS ICP Deep Reactive Ion Etcher. Have noticed that the APC angle
is slightly different in different protocols and this seems to affect the etch
outcome. Could I ask what is APC angle and how does it affect etch profile and
speed. Thanks.

Regards,
Melissa


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list options,
visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services. Visit us at
http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
MEMS Technology Review
The Branford Group