PEYRADE David
2004-02-04
Reiner Witte
2004-02-05
Josef Kouba
2004-02-04
Jan Friday
Glass substrate supplier
PEYRADE David
2004-02-04
Dear MEMS researchers,

I am looking for 200mm or100mm glass substrate that transmit 80% of light at
193nm.
Does anyone know which kind of glass must be used ?
Do you know a supplier for this kind of product ?

Thanks a lot.

________________________

David PEYRADE

CNRS-LTM
CEA LETI
Bat.4120 p 220
17, rue des Martyrs
38054 Grenoble Cedex 9
Bat4120 Pièce 204
Tel:  33 (0)4 38 78 38 82
Fax:  33 (0)4 38 78 58 92
________________________


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMStaff Inc.