MEMSnet Home: MEMS-Talk: Glass substrate supplier
Glass substrate supplier
2004-02-04
PEYRADE David
2004-02-04
Reiner Witte
2004-02-05
Josef Kouba
2004-02-04
Jan Friday
Glass substrate supplier
Josef Kouba
2004-02-05
F-doped quarz glass will work fine (transmitts as deep as 157 nm).
I only know one company in Germany called SCHOTT, but search simply in
internet, there will be more of them since 193nm and 157nm are commonly
beeing used.

Josef Kouba
BESSY GmbH, AZM Group
Albert Einstein Str. 15
D-12489 Berlin
Tel.: +49-30-6392-3125
Fax: +49-30-6392-4682
email: [email protected]
www: www.azm.bessy.de







----- Original Message -----
From: "PEYRADE David" 
To: 
Sent: Wednesday, February 04, 2004 3:48 PM
Subject: [mems-talk] Glass substrate supplier


> Dear MEMS researchers,
>
> I am looking for 200mm or100mm glass substrate that transmit 80% of light
at
> 193nm.
> Does anyone know which kind of glass must be used ?
> Do you know a supplier for this kind of product ?
>
> Thanks a lot.
>
> ________________________
>
> David PEYRADE
>
> CNRS-LTM
> CEA LETI
> Bat.4120 p 220
> 17, rue des Martyrs
> 38054 Grenoble Cedex 9
> Bat4120 Pièce 204
> Tel:  33 (0)4 38 78 38 82
> Fax:  33 (0)4 38 78 58 92
> ________________________
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
The Branford Group
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics