Preparation of KI+I2+DIwater solution for gold etching
2004-02-08
hare krishna
2004-02-09
aasutosh dave
SU8 Information
2004-02-10
[email protected]
2004-02-10
Samir Kagadkar
SU-8 adhesion problem
2004-02-11
[email protected]
2004-02-11
Karin Buchholz
2004-02-12
Greg Reimann
Polishing service
2004-02-16
Changping LUO
2004-02-10
hare krishna
TLM structure for measuring the specific contact resistance
2004-02-11
hare krishna
2004-02-29
hare krishna
2004-02-16
aasutosh dave
TLM structure for measuring the specific contact resistance
hare krishna
2004-02-11
Dear All,
             Can anybody suggest me the dimensions for the TLM mask(Transmission
Line Method) that is the width of contact and the separation between  them, used
for the measurement of specific contact resistance by  photolithography process.

Hare Krishna

hare krishna  wrote:
Dear Dave,
Thanks for your reply but sir, I also want to know about the solution making
procedure because last time I just mixed the KI and I2 powders and made the
solution with DI water, which is not the correct way of making the solution
because Iodine is very volatile.

Hare Krishna

aasutosh dave wrote:
Hare Krishna,

I use 20gm KI : 5gm Iodine : 160 ml DI water. You can change the
concentration too to achieve higher etch rates. If you want you can reuse it
for few times but not more as you will notice the etch rate will change each
time you resue it. As far as I know you can preserve in any sealed glass or
plastic bottle.

Regards,

Aasutosh Dave

Nanofab Center
Arlington, Texas


>From: hare krishna
>Reply-To: General MEMS discussion
>To: [email protected]
>Subject: [mems-talk] Preparation of KI+I2+DIwater solution for gold etching
>Date: Sun, 8 Feb 2004 05:47:03 +0000 (GMT)
>
>
>Dear All,
> How should I make the solution of KI + I2 + DI water for the
>gold etching. Should I use it fresh or I can use it for long time...and how
>should it be preserved.
>Regards
>Hare Krishna
>
>
>
>Yahoo! India Education Special: Study in the UK now.
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/

_________________________________________________________________
Let the advanced features & services of MSN Internet Software maximize your
online time. http://click.atdmt.com/AVE/go/onm00200363ave/direct/01/


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
Yahoo! India Education Special: Study in the UK now.
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
Yahoo! India Education Special: Study in the UK now.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Tanner EDA by Mentor Graphics
University Wafer