MEMSnet Home: MEMS-Talk: Preparation of KI+I2+DIwater solution for gold etching
SU8 Information
2004-02-10
[email protected]
2004-02-10
Samir Kagadkar
SU-8 adhesion problem
2004-02-11
[email protected]
2004-02-11
Karin Buchholz
2004-02-12
Greg Reimann
Polishing service
2004-02-16
Changping LUO
Preparation of KI+I2+DIwater solution for gold etching
2004-02-10
hare krishna
TLM structure for measuring the specific contact resistance
2004-02-11
hare krishna
2004-02-11
Brubaker Chad
Preparation of KI+I2+DIwater solution for gold etching
2004-02-29
hare krishna
2004-03-01
Customer Service
Preparation of KI+I2+DIwater solution for gold etching
hare krishna
2004-02-29
Dear Dave,
             Can I use the prepared KI,I2,DI water (4:1:40) solution for gold
etchant after 20 days because I preserved it in a glass bottle.

Regards
Hare Krishna


aasutosh dave  wrote:
Hare Krishna,

I use 20gm KI : 5gm Iodine : 160 ml DI water. You can change the
concentration too to achieve higher etch rates. If you want you can reuse it
for few times but not more as you will notice the etch rate will change each
time you resue it. As far as I know you can preserve in any sealed glass or
plastic bottle.

Regards,

Aasutosh Dave

Nanofab Center
Arlington, Texas


>From: hare krishna
>Reply-To: General MEMS discussion
>To: [email protected]
>Subject: [mems-talk] Preparation of KI+I2+DIwater solution for gold etching
>Date: Sun, 8 Feb 2004 05:47:03 +0000 (GMT)
>
>
>Dear All,
> How should I make the solution of KI + I2 + DI water for the
>gold etching. Should I use it fresh or I can use it for long time...and how
>should it be preserved.
>Regards
>Hare Krishna
>
>
>
>Yahoo! India Education Special: Study in the UK now.
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/

_________________________________________________________________
Let the advanced features & services of MSN Internet Software maximize your
online time. http://click.atdmt.com/AVE/go/onm00200363ave/direct/01/


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/
Yahoo! India Insurance Special: Be informed on the best policies, services,
tools and more.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
Addison Engineering
MEMStaff Inc.