MEMSnet Home: MEMS-Talk: Preparation of KI+I2+DIwater solution for gold etching
Preparation of KI+I2+DIwater solution for gold etching
2004-02-16
aasutosh dave
2004-02-29
hare krishna
2004-03-01
Customer Service
2004-03-02
aasutosh dave
Preparation of KI+I2+DIwater solution for gold etching
aasutosh dave
2004-03-02

>Dear Dave,
>              Can I use the prepared KI,I2,DI water (4:1:40) solution for
>gold etchant after 20 days because I preserved it in a glass bottle.
>
>Regards
>Hare Krishna
>


Hare Krishna,

You can use the solution for more than 20 days unless the bottle was opened.
The solution will be diluted after few cycles which results in nothing but
some more etching time. I generally use the solution for like 4 - 6 months.


Regards,

Aasutosh Dave

_________________________________________________________________
Get a FREE online computer virus scan from McAfee when you click here.
http://clinic.mcafee.com/clinic/ibuy/campaign.asp?cid=3963



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Addison Engineering
MEMStaff Inc.