MEMSnet Home: MEMS-Talk: Electroless nickel/Immersion gold process
Electroless nickel/Immersion gold process
2004-03-11
Tanya Snyder
2004-03-15
Dr. Hermann Oppermann
2004-03-15
David Nemeth
Electroless nickel/Immersion gold process
Tanya Snyder
2004-03-11
Could anyone recommend a reference containing a process for plating
electroless nickel and immersion gold?

Thanks,
Tanya Snyder
MicroHouse Technologies
[email protected]