MEMSnet Home: MEMS-Talk: Electroless nickel/Immersion gold process
Electroless nickel/Immersion gold process
2004-03-11
Tanya Snyder
2004-03-15
Dr. Hermann Oppermann
2004-03-15
David Nemeth
Electroless nickel/Immersion gold process
Dr. Hermann Oppermann
2004-03-15
Dear Tanya,

please visit the download area of my collegue Andreas Ostmann who is
working since more than ten years in electroless nickel / immersion gold
plating on CMOS wafers:

http://www.pb.izm.fhg.de/avt/050_download/index.html

regards,

Hermann

Tanya Snyder wrote:

>Could anyone recommend a reference containing a process for plating
>electroless nickel and immersion gold?
>
>Thanks,
>Tanya Snyder
>MicroHouse Technologies
>[email protected]
>
>
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/
>
>
>
>
>

--
Dr. Hermann Oppermann
Fraunhofer IZM
Gustav-Meyer-Allee 25
D-13355 Berlin, Germany
----------------------------------------------------------
phone: +49-30-46403-163, -153 (secr.)
Fax:   +49-30-46403-162
email: [email protected]
----------------------------------------------------------
Dept. Photonic and Power System Assembly
Group Optoelectronics System Integration
http://www.izm.fhg.de/avt/opperm.htm
----------------------------------------------------------

"Diese E-Mail kann Betriebs- und Geschäftsgeheimnisse, dem Anwaltsgeheimnis
unterliegende oder sonstige vertrauliche Informationen enthalten. Sollten Sie
diese E-Mail irrtümlich erhalten haben, ist Ihnen die Kenntnisnahme des Inhalts,
eine Vervielfältigung oder Weitergabe der E-Mail ausdrücklich untersagt. Bitte
benachrichtigen Sie den Absender der E-Mail und vernichten die empfangene
E-Mail. Vielen Dank."

"Since this e-mail contains confidential information, it must be treated with
utmost confidentiality. Any person who may get in contact with this information
by mistake should not take any notice of the topic and should not pass on or
duplicate any part of this informatio
n. The e-mail has to be destroyed and the sender of the the e-mail has to be
informed immediately. Thank you."




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
Mentor Graphics Corporation
Harrick Plasma, Inc.