MEMSnet Home: MEMS-Talk: fabricating optics with reflowed photoresist in plasma etcher, problem with surface roughness
fabricating optics with reflowed photoresist in plasma etcher, problem with surface roughness
2004-04-04
Patrick Lu
CORRECTION: fabricating optics with reflowed photoresist in plasmaetcher, problem with surface roughness
2004-04-05
Patrick Lu
fabricating optics with reflowed photoresist in plasma etcher, problem with surface roughness
Patrick Lu
2004-04-04
Hi,



I have quartz wafers covered with reflowed photoresist. I am etching these
with a mixed CH4 and O2 plasma. Hopefully, I will be able to adjust the
height of the resulting optic by changing the gas concentrations (with CH4
etching the glass and O2 etching the photoresist). Right now, the optics
that come out of the plasma etcher are very rough-much rougher than the
photoresist profiles that shaped them. Under a microscope, I see many cracks
in the surface of the quartz. The "bumpiness" is on the order of 1/3 of a
micron (where the optic height is 1 - 2 microns). I am running at a pressure
of 150 mTorr, with gas flow rates of 100 cc/m for CH4 and 50 cc/m for O2,
and 83 W of RF power. If anyone has experience etching glass with reflowed
photoresist, their advice would be much appreciated!



Thanks!



Patrick Lu

Stanford University

Department of Electrical Engineering

http://www.stanford.edu/~patlu


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer
MEMStaff Inc.