Ti RIE
2004-04-15
Greg Chance
2004-04-21
Jason Viotty
Ti RIE
Greg Chance
2004-04-15
Hi everyone

Would anyone be able to tell me the recipe for dry etching titanium, i.e.
what gas, pressure, plate etc? I need to etch 200 nm which has been
evaporated on a GaAs substrate.

regards
Greg Chance
Bath University Physics Dept.