Nickel etchant
2004-05-07
Sandy Kumar
2004-05-10
Customer Service
sputtering of Ti on polymer substrate
2004-05-11
Robert Dean
2004-05-10
Greg Chance
Nickel etchant
Customer Service
2004-05-10
Sandy--

Transene Company (www.transene.com) manufactures Nickel Etch TFG for
selectively etching nickel in the presence of copper.

Christopher Christuk
Transene Company


> I am looking for a chemical wet process etchant to etch nickel from copper
substrate. Nickel is about 200 microinch thick plating. Could anyone please
help?
>
> Thanks.
> Sandy
>
>
>
>
>
> ---------------------------------
> Do you Yahoo!?
> Win a $20,000 Career Makeover at Yahoo! HotJobs
>



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Addison Engineering
The Branford Group
Process Variations in Microsystems Manufacturing