MEMSnet Home: MEMS-Talk: sputtering of Ti on polymer substrate
Nickel etchant
2004-05-07
Sandy Kumar
2004-05-10
Customer Service
sputtering of Ti on polymer substrate
2004-05-11
Robert Dean
2004-05-10
Greg Chance
sputtering of Ti on polymer substrate
Robert Dean
2004-05-11
Hello,

Can anyone recommend a vender that can Ar ion clean a polymer substrate and
then deposit a thin layer of Ti by sputtering?  Please respond to my email
address directly.

Sincerely,

Robert Dean

Research Associate IV
Center for Advanced Vehicle Electronics
Auburn University
200 Broun Hall
Auburn, AL 36849

Voice: 334-844-1838
Fax:   334-844-1898
Email: [email protected]
Web: http://www.eng.auburn.edu/~deanron



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing