Chromium etchant selective to copper
2004-08-10
Shweta Humad
2004-08-11
Greg Reimann
2004-08-12
David
SU-8 Density?
2004-08-14
Siripon Sukuabol
2004-08-15
Christopher Blanford
Piezoelectric Beam Simulation by using Ansys
2004-08-16
Siripon Sukuabol
Removal of reflowed AZ resist
2004-08-16
Erik Jung
2004-08-16
Michael Cooke
2004-08-17
Kirt Williams
2004-08-18
Michael D Martin
2004-08-18
Park, Daniel Sang-Won
Chromium etchant selective to copper
Greg Reimann
2004-08-11
Shweta,

This is probably not what you are looking for, but I'm using a Cl-O2
plasma etch for Chrome over Copper, The copper surface forms a Chloride
which needs to be washed away in a dilute HCl dip but is otherwise
untouched.  It might be worth a shot.

Greg
Boston U.

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Shweta Humad
Sent: Tuesday, August 10, 2004 5:58 PM
To: [email protected]
Subject: [mems-talk] Chromium etchant selective to copper


Does anyone know of a chromium etchant selective to copper?

Thanks,
--
Shweta Humad



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Nano-Master, Inc.
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing