MEMSnet Home: MEMS-Talk: Removal of reflowed AZ resist
Chromium etchant selective to copper
2004-08-10
Shweta Humad
2004-08-11
Greg Reimann
2004-08-12
David
SU-8 Density?
2004-08-14
Siripon Sukuabol
2004-08-15
Christopher Blanford
Piezoelectric Beam Simulation by using Ansys
2004-08-16
Siripon Sukuabol
Removal of reflowed AZ resist
2004-08-16
Erik Jung
2004-08-16
Michael Cooke
2004-08-17
Kirt Williams
2004-08-18
Michael D Martin
2004-08-18
Park, Daniel Sang-Won
Removal of reflowed AZ resist
Michael Cooke
2004-08-16
I dont have experience of this exactly, but you could imerse it in bomb if
your other components will hold
Dr. Michael Cooke
Microsystems Technology Group
School Of Engineering
University of Durham
Durham
DH1 3LE
Phone: +44 (0)191 3342535
Fax:      +44 (0)191 3342407
Email:   [email protected]
Webpage Http://www.dur.ac.uk/microsystems.technology
----- Original Message -----
From: "Erik Jung" 
To: "General MEMS discussion" 
Sent: Monday, August 16, 2004 10:25 AM
Subject: [mems-talk] Removal of reflowed AZ resist


> Dear all,
> anyone of you has experience in completely removing AZ photoresist after
> reflowing SnAg solder in the openings (Tmax~230?C, t@Tmax ~ 40sec)
> Thank you!
>
> Erik
> TU Berlin
>
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation