A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Regd KOH Bath Temperature Tolerance
Regd KOH Bath Temperature Tolerance
2004-10-05
guda reddy
2004-10-06
Keith Jackson
Regd KOH Bath Temperature Tolerance
guda reddy
2004-10-05
Hi,

 I would like to know what could be the allowed temperature tolerance for the
KOB bath used for etching silicon, as we cannot maintain the bath exactly at one
particular temperature as it keeps fuctuating around 2-3 degrees.
I would really appreciate if you could reply.

Thanks,
dhanamjaya
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
University Wafer
Process Variations in Microsystems Manufacturing