Regd KOH Bath Temperature Tolerance
2004-10-05
guda reddy
2004-10-06
Keith Jackson
Regd KOH Bath Temperature Tolerance
Keith Jackson
2004-10-06
I have been using 85 C as a bath temp. with 0.1 degree control
Keith Jackson
----- Original Message -----
From: "guda reddy" 
To: "General MEMS discussion" 
Sent: Tuesday, October 05, 2004 2:32 PM
Subject: [mems-talk] Regd KOH Bath Temperature Tolerance


> Hi,
>
>  I would like to know what could be the allowed temperature tolerance for
the KOB bath used for etching silicon, as we cannot maintain the bath
exactly at one particular temperature as it keeps fuctuating around 2-3
degrees.
> I would really appreciate if you could reply.
>
> Thanks,
> dhanamjaya
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Harrick Plasma, Inc.