A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: gold, photoresist, UV light, bubbles
gold, photoresist, UV light, bubbles
2004-11-29
Rick Giuly
2004-11-29
Z.,W.Y.(Lydia)
2004-11-30
Brad Cantos
2004-11-30
Marco Doms
gold, photoresist, UV light, bubbles
Brad Cantos
2004-11-30
Rick:
The photochemical reaction of novalac-based positive resist causes nitrogen
to be evolved during exposure.  If the bubbles form only when photoresist is
present, then it is likely that this is the source of your gas bubbles.  One
way to eliminate the bubbles is to reduce the exposure intensity while
keeping the dose constant.  This will give the nitrogen more time to migrate
through the thick resist layer.  I have used a pulse exposure technique in
the past, with a 20-30% duty cycle.
Brad

On 11/28/04 7:56 PM, "Rick Giuly"  wrote:

> Hello All,
>
> Listed from top to bottom, I have these layers:
> 8 micron AZ P4620 photoresist (spun on)
> ..5 micron gold (ebeam at ~10e-6 torr, 5A per sec)
> 10 micron PDMS (spun on)
> glass substrate
>
> When I expose with UV light, gas bubbles form between the gold and the
> PDMS. They do not form if there is no photoresist.
>
> Any ideas on where the bubbles come from and how to get rid of them?
>
>
> -Rick Giuly
> GA Tech
>
>
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
University Wafer
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.