gold, photoresist, UV light, bubbles
Marco Doms
2004-11-30
Rick,

during exposure, the photo active compound of photoresist converts into a
carboxylic acid seperating a N2 molecule. Your bubbles probably are caused
by this nitrogen generation. Try to expose the resist prior to depositing
another layer on top of it (after a sufficiently long softbake) to ensure
that all the nitrogen can diffuse from the resist layer before you
hermetically seal it.

Marco

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
MEMS Technology Review
University Wafer