MEMSnet Home: MEMS-Talk: Metalic vs poly heaters
Metalic vs poly heaters
2005-02-03
Stephen Arnold
2005-02-03
Kirt Williams
2005-02-04
Michael D Martin
Metalic vs poly heaters
Stephen Arnold
2005-02-03
We have a design idea which would require a high temperature source
(~1100 deg.C). We are deciding between highly doped (10^20) polysilicon
heaters or refractory(W, Ta) or other (Pt) metal heaters. The heater is
to be encased in SiO2 (sputtered) and we are concerned with the high TCE
differences between the metal and the SiO2. For this reason, we are
leaning towards the poly-heater approach, but if anyone in the community
would like to share some of there experience, it would be greatly
appreciated. Thanks.

Steve

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
University Wafer