Stephen Arnold
2005-02-03
Kirt Williams
2005-02-04
Michael D Martin
Metalic vs poly heaters
Kirt Williams
2005-02-03
Around 1989, Carlos Mastangelo made freestanding polysilicon heaters coated
with silicon nitride.
These were heated to at least a dim red hot (probably over 900 C), but I
don't know the temperature-lifetime characteristics.
Check on his disseration (U.C. Berkeley) and papers.

Yes, tungsten heaters need some type of protection to survive in air.
Platinum, being a noble metal, has been used for heaters in contact with air
without a coating.
NiCr and TaN are other candidates that may not need protection at 1100 C.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing