Any metal as KOH masking layer?
2005-06-02
Joe Lonjin
2005-06-03
Joe Lonjin
2005-06-08
Nickolai Belov
Any metal as KOH masking layer?
Joe Lonjin
2005-06-02
Why metal? Use Nitride or get Protek from Brewer Science.

Joe Lonjin
Penn State Nanofabrication Facility
College of Engineering

-----Original Message-----
From: D. Zhou [mailto:[email protected]]
Subject: [mems-talk] Any metal as KOH masking layer?

I am just wondering if any metal can act as the masking layer( strong
enough in KOH and easy to be removed) for deep KOH etching (say,~600 um
deep) at 80 degrees. (It may take about 10 hours to finish the etching
process). I tried NiCr (50 nm) but it could not sustain after 2 hours.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMStaff Inc.