Hello Daxiang,

There are several options to address the issue.
You can try copper or gold.  These metals stay in KOH.
Nickel is also a good mask in KOH.
However, masking layer should be thicker than what you are using.

It is important to have a masking sub-layer as well. Otherwise, KOH will
penetrate through metal layer via pinholes or places with poor adhesion
and form cavities under the mask.

With respect

Nickolai Belov
Nanochip, Inc.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
Addison Engineering
Harrick Plasma, Inc.