MEMSnet Home: MEMS-Talk: contamination after KOH etching
contamination after KOH etching
2005-06-23
Bo He
2005-06-24
Dan.W.Chilcott
2005-06-25
Michael L
contamination after KOH etching
Dan.W.Chilcott
2005-06-24
Bo-
It is possible to oxidize the nickel in KOH. Nickel oxide can be difficult to
remove. I do not have a process for removing the oxide but the oxide can be
altered by changing the bath temperature and concentration.

Dan Chilcott
MEMS Advanced Development
Delphi Corporation

 -----Original Message-----
From:   [email protected] [mailto:[email protected]]  On
Behalf Of Bo He
Sent:   Thursday, June 23, 2005 12:49 PM
To:     [email protected]
Subject:        [mems-talk] contamination after KOH etching

Dear All:

       Our substrate is electroplated Ni and PVD Ni on silicon. After KOH
etching of Si, the Ni surface looks "yellowlish" and we have tried using
different kinds of acids(hcl,h2so4,hno3) to remove this contamination but
neither works. Any suggestions?

Many thanks.

Bo


_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk



********************************************************************************
********

Note: The information contained in this message may be privileged and
confidential and thus protected from disclosure. If the reader of this message
is not the intended recipient, or an employee or agent responsible for
delivering this message to the intended recipient, you are hereby notified that
any dissemination, distribution or copying of this communication is strictly
prohibited. If you have received this communication in error, please notify us
immediately by replying to the message and deleting it from your computer. Thank
you.

********************************************************************************
********
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
MEMStaff Inc.
University Wafer