MEMSnet Home: MEMS-Talk: contamination after KOH etching
contamination after KOH etching
2005-06-23
Bo He
2005-06-24
Dan.W.Chilcott
2005-06-25
Michael L
contamination after KOH etching
Michael L
2005-06-25
Hi Bo,

How about plating a protective layer (such as Au or Cr) onto the Ni and
removing this via wet etching after the KOH step?

Michael