A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Thin PDMS Films
Reg: problems with SU-8 bonding to the silicon wafer
2005-06-23
Vishwanath Somashekar
2005-06-23
[email protected]
2005-06-23
Vishwanath Somashekar
Thin PDMS Films
2005-06-24
[email protected]
2005-06-25
Tolga Kaya
2005-06-27
Patrick Roman
2005-06-23
Brubaker Chad
2005-06-24
Brubaker Chad
2005-06-27
Vishwanath Somashekar
2005-06-29
Brubaker Chad
2005-06-30
Vishwanath Somashekar
Thin PDMS Films
Tolga Kaya
2005-06-25
Hi, I am not sure I understand you clearly but I tried before to spin
PDMS on Si molds. If you use TMCS or any kind of silanization, you can
easily detach your thin film PDMS. If your thin film PDMS is on the
order of 10um, it is going to be a very thin membrane and you will not
be able to detach in a single piece. You can put a thick PDMS on it
after plasma treatment and yoy can easily detach it from your
substrate without breaking.

I hope it works for you.

Tolga

On 6/24/05, [email protected]  wrote:
> Hi all,
>
> I was wondering if anyone has experience casting thin films of PDMS by
> clamping down the mold in order to get a film that is as thick as the features
> on the mold. If so, does anyone have suggestions/tips on removing the film
> from the mold once it's done? I've been having trouble with tearing the film
> as I try to peel it off by hand.
>
> thanks,
> Joe Grogan
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
The Branford Group
Nano-Master, Inc.