Dear all:
   Now I`m try to do some hydrophilic bonding.At first, Si wafers are cleaned by
standard RCA1.But even after treated by
HNO3+HF(65%HNO3:48%HF:H2O=5:100:0.001),Si wafers do not wettable.Is the recipe
right? Please help me!Thanks a lot.
                                                       Nielei



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation