MEMSnet Home: MEMS-Talk: Gold etching (Nik Dee)
Gold etching (Nik Dee)
2005-07-18
Nik Dee
2005-07-18
Shile
2005-07-25
David Nemeth
Gold etching (Nik Dee)
Nik Dee
2005-07-18
Hi guys, I have been using HCl (hydrochloric) and NaCl (nitric) acid to etch the
gold away. I recently realised that if there is copper in the sample the acid
attacks the copper and has no affect on the gold surface anymore. Does anybody
know any etching recipe that i can remove the gold without affecting the
copper?


Nik Dee


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
University Wafer