MEMSnet Home: MEMS-Talk: Gold etching (Nik Dee)
Gold etching (Nik Dee)
2005-07-18
Nik Dee
2005-07-18
Shile
2005-07-25
David Nemeth
Gold etching (Nik Dee)
Shile
2005-07-18
NaCl is sodium chloride, not nitric acid. And it doesn't etch gold.
(Otherwise there wouldn't be any pirates' booty left on the sea floor.)

Roger Shile

-----Original Message-----
From: Nik Dee
Subject: [mems-talk] Gold etching (Nik Dee)

Hi guys, I have been using HCl (hydrochloric) and NaCl (nitric) acid to
etch the
gold away. I recently realised that if there is copper in the sample the
acid
attacks the copper and has no affect on the gold surface anymore. Does
anybody
know any etching recipe that i can remove the gold without affecting the
copper?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group
Addison Engineering