Hi,
I have a Alcatel pump neeed to use Fomblin oil. However, I wrongfully used
general mechanic pump oil(fishbrand 19) for a while. Until I find the
capacity is lower.....
I am really new in vacum area. Would you please give me any suggestion on
this issue now? Need to send back or some pump service company for cleaning?
Or I can just drain the oil out and add new Formbin oil?
Thanks a lot
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMStaff Inc.