MEMSnet Home: MEMS-Talk: wrong pump oil used
wrong pump oil used
2006-02-12
shenghong qiu
2006-02-13
Dave Freedman
2006-02-13
[email protected]
wrong pump oil used
[email protected]
2006-02-13
A mechanical pump must be either a corrosive series pump or just a pump
made for mech oil.  To use Fomblin, the pump must be "Fomblin prepped".
This means the seals in the pump are made for Fomblin oil or corrosive
service.  Now that you have used regular mechanical pump oil, the pump must
now be sent out to be cleaned and if it is not a corrosive series pump, it
must be rebuilt.  Many companies do this work for around $1100.  Write me
if you
want the name of a good pump rebuilder.

Brent

Original Message:
-----------------
From: shenghong qiu [email protected]
Date: Sat, 11 Feb 2006 22:12:27 -0500
To: [email protected]
Subject: [mems-talk] wrong pump oil used


Hi,
I have a Alcatel pump neeed to use Fomblin oil. However, I wrongfully used
general mechanic pump oil(fishbrand 19) for a while. Until I find the
capacity is lower.
I am really new in vacum area. Would you please give me any suggestion on
this issue now? Need to send back or some pump service company for cleaning?
Or I can just drain the oil out and add new Formbin oil?
Thanks a lot
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
University Wafer
Process Variations in Microsystems Manufacturing