Any ways to minimize the writing times for Heidelberg DWL66 mask maker?
2006-02-17
Chih-Chieh Cheng
Any ways to minimize the writing times for HeidelbergDWL66 mask maker?
2006-02-21
David Nemeth
2006-02-21
Gareth Jenkins
Any ways to minimize the writing times for Heidelberg DWL66 mask maker?
Chih-Chieh Cheng
2006-02-17
Hi, everyone

As title, we are seeking a way to minimize the writing times because of the
cost issue. Our cleanroom charges per hour for Heidelberg. Anyone has any
ideas?

Thanks

Chih-Chieh
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Addison Engineering
Mentor Graphics Corporation
MEMS Technology Review