MEMSnet Home: MEMS-Talk: Any ways to minimize the writing times for HeidelbergDWL66 mask maker?
Any ways to minimize the writing times for Heidelberg DWL66 mask maker?
2006-02-17
Chih-Chieh Cheng
Any ways to minimize the writing times for HeidelbergDWL66 mask maker?
2006-02-21
David Nemeth
2006-02-21
Gareth Jenkins
Any ways to minimize the writing times for HeidelbergDWL66 mask maker?
David Nemeth
2006-02-21
Chih-Chieh,

I would encourage you to look at commercial mask vendors as well. I don't
know if it would actually come out to be cheaper or not, and it would depend
on a variety of factors, but if you get optically printed masks on soda lime
substrates, they aren't terribly expensive.

Type "photomask" into google.com to pull up a list of vendors.

David Nemeth
Senior Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA 20151


-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Chih-Chieh Cheng
Sent: Friday, February 17, 2006 11:41 AM
To: [email protected]
Subject: [mems-talk] Any ways to minimize the writing times for
HeidelbergDWL66 mask maker?


Hi, everyone

As title, we are seeking a way to minimize the writing times because of the
cost issue. Our cleanroom charges per hour for Heidelberg. Anyone has any
ideas?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Mentor Graphics Corporation
University Wafer
Nano-Master, Inc.