Is there any way to etch a hole through on silicon wafer?
2006-04-03
Jeff chen
Is there any way to etch a hole through on siliconwafer?
2006-04-03
Shile
Is there any way to etch a hole through on silicon wafer?
2006-04-03
Florian Herrault
Is there any way to etch a hole through on silicon wafer?
2006-04-07
Leo Petrossian
native silicon oxide growth rate
2006-04-09
li cai
2006-04-10
Duan
Is there any way to etch a hole through on silicon
2006-04-04
Carel Heerkens
Is there any way to etch a hole through on silicon
Carel Heerkens
2006-04-04
DRIE etching using Bosch ICP or Cryo ICP will do the trick. aspect ratio
of up to 10 is feasible. The choice depends on availability and mask
design and -material.
greetings Carel

Jeff chen wrote:

>Hi,
>
>I am working on a project which needs to etch a hole through the
>silicon wafer (525 micron thick). The hole diameter is around 50
>micron.
>Does anyone have experience to do that?
>Is there any way to do that? Etching? Laser excimer? or grounding
>technology?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Mentor Graphics Corporation
MEMS Technology Review
Addison Engineering