MEMSnet Home: MEMS-Talk: native silicon oxide growth rate
Is there any way to etch a hole through on silicon wafer?
2006-04-03
Jeff chen
Is there any way to etch a hole through on siliconwafer?
2006-04-03
Shile
Is there any way to etch a hole through on silicon wafer?
2006-04-03
Florian Herrault
Is there any way to etch a hole through on silicon wafer?
2006-04-07
Leo Petrossian
native silicon oxide growth rate
2006-04-09
li cai
2006-04-10
Duan
Is there any way to etch a hole through on silicon
2006-04-04
Carel Heerkens
native silicon oxide growth rate
Duan
2006-04-10
check this website:
http://snf.stanford.edu/Process/Characterization/NativeOx.html

On 4/9/06, li cai  wrote:
> Does anyone knows the growth rate of native silicon oxide?

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer
Addison Engineering