etch stop layers for silicon DRIE
2008-11-13
Sebastian Sosin
2008-11-13
Henk van Zeijl
2008-11-13
Xiaoguang Liu
2008-11-14
Vijay Rajaraman
2008-11-14
汪飞
2008-11-17
Sebastian Sosin
etch stop layers for silicon DRIE
Henk van Zeijl
2008-11-13
Hi Sebastian

How about ALD deposited Al2O3, it is deposited at low temperature, conformal
and the etch-rate in silicon DRIE is very low. If I'm correct, selectivities
of 1:10000 are reported.

Kind regards, Henk van Zeijl

Delft University of Technology / DIMES
POBox 5053
NL-2600 GB  DELFT
The Netherlands
phone: ++31 15 2781092
fax:   ++31 15 2787369
Email: [email protected]
http://www.dimes.tudelft.nl

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Sebastian Sosin
Sent: 13 November 2008 15:38
To: [email protected]
Subject: [mems-talk] etch stop layers fro silicon DRIE

Does anyone have any knowledge of other etch stop layers for silicon DRIE,
besides SiO2 and Al? We have an Adixen system and for my process it would
save extra work to have something else as etch stop layer (not Al or SiO2).

Sebastian Sosin
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer