MEMSnet Home: MEMS-Talk: etch stop layers for silicon DRIE
etch stop layers for silicon DRIE
2008-11-13
Sebastian Sosin
2008-11-13
Henk van Zeijl
2008-11-13
Xiaoguang Liu
2008-11-14
Vijay Rajaraman
2008-11-14
汪飞
2008-11-17
Sebastian Sosin
etch stop layers for silicon DRIE
Sebastian Sosin
2008-11-17
Yes, through the wafer, 525 microns deep

__________________________________________________________________

Sebastian Sosin


-----Original Message-----

From: 汪飞 [mailto:[email protected]]
Sent: Friday, November 14, 2008 1:58 PM
To: General MEMS discussion
Subject: Re: [mems-talk] etch stop layers fro silicon DRIE

Do you want etch through a wafer?



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
The Branford Group
MEMS Technology Review
Nano-Master, Inc.