selective negative resist stripper
2008-11-17
Javier Crespo
2008-11-17
Bill Moffat
2008-11-19
Jason Milne
2008-11-19
Avi Laker
selective negative resist stripper
Bill Moffat
2008-11-17
Oxygen plasma with or without the addition of a small amount of CF4 or
SF6.  Bill Moffat

________________________________

From: [email protected] on behalf of Javier Crespo
Sent: Mon 11/17/2008 7:42 AM
To: [email protected]
Subject: [mems-talk] selective negative resist stripper

Dear All,

Could anyone tell me how could I remove negative photoresist from a
silicon wafer without affecting metal layer (Ni or AlSi)?

I know that the piranha etching etches the resist in a higher rate than
the metal, but I don't know in which percentage.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Nano-Master, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing