MEMSnet Home: MEMS-Talk: selective negative resist stripper
selective negative resist stripper
2008-11-17
Javier Crespo
2008-11-17
Bill Moffat
2008-11-19
Jason Milne
2008-11-19
Avi Laker
selective negative resist stripper
Avi Laker
2008-11-19
 If ther resist is not to thick you may try an O2 plasma - it's very
slow.
 There are strippers - expensive - to strip negattive resist by several
 manufactures.

-
   1. selective negative resist stripper (Javier Crespo)


Message: 1
Date: Mon, 17 Nov 2008 16:42:57 +0100
From: "Javier Crespo" 
Subject: [mems-talk] selective negative resist stripper
To: 
Message-ID:

<2320FF588EF2E34AA1F756CB6284ECBD04BDFF8B@srvcorreo.fagorelectronica.es>

Content-Type: text/plain;       charset="us-ascii"

Dear All,

Could anyone tell me how could I remove negative photoresist from a
silicon wafer without affecting metal layer (Ni or AlSi)?

I know that the piranha etching etches the resist in a higher rate than
the metal, but I don't know in which percentage.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Addison Engineering
The Branford Group
MEMS Technology Review