SU-8 removal
Don Friedrich
2008-12-11
We have the same problem using essentially the same process.  We don't
do electroplating, but the 200 deg cured SU-8, 10 um thick, does not
release from the OmniCoat.  We tried warm NanoRemover PG in ultrasonic
bath for several hours.  The OmniCoat layer is 20-30 nm thick using
MicroChem recommended spin process.  We thick this is too thin.  What
methods will spin coat thicker layers of OmniCoat?  What process would
increase OmniCoat viscosity?

Don Friedrich
Research & Development
JDSU - Advanced Optical Technologies

2789 Northpoint Parkway, M.S. BF-1
Santa Rosa, CA 95407 USA
707-525-7258 (Voice)
[email protected]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
Process Variations in Microsystems Manufacturing
MEMS Technology Review