SU-8 removal
Hennemeyer, Marc
2008-12-12
Hi Don,

some time ago I had a discussion about this topic at a conference. The
guy I was talking to had good experience with multiple Omnicoat coating
steps, perhaps 3 or 4 layers. I never tried it myself, though.

Marc Hennemeyer
_________________________________
Application Engineer
SUSS MicroTec Lithography GmbH
phone +49-(0) 89-32007-128



-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Don Friedrich
Sent: Thursday, December 11, 2008 11:51 PM
To: General MEMS discussion
Subject: [mems-talk] SU-8 removal

We have the same problem using essentially the same process.  We don't
do electroplating, but the 200 deg cured SU-8, 10 um thick, does not
release from the OmniCoat.  We tried warm NanoRemover PG in ultrasonic
bath for several hours.  The OmniCoat layer is 20-30 nm thick using
MicroChem recommended spin process.  We thick this is too thin.  What
methods will spin coat thicker layers of OmniCoat?  What process would
increase OmniCoat viscosity?

Don Friedrich
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.