MEMSnet Home: MEMS-Talk: Looking for vendors/services for HDP-CVD of Silicon Nitride
Looking for vendors/services for HDP-CVD of Silicon Nitride
2009-04-17
Harshal Surangalikar
2009-04-17
Pat Kayatta
2009-04-20
Glenn Silveira
Looking for vendors/services for HDP-CVD of Silicon Nitride
Pat Kayatta
2009-04-17
Hello Harshal,

PECVD films processed at temperatures of 350C and higher generally provide a
higher etch resistance than those processed at lower temperature.

I would consider PECVD Silicon Carbide, as this film not only provides
excellent etch resistance to HF & BOE, but to KOH as well.

Best Regards,

Pat Kayatta
Rogue Valley Microdevices
943 Automation Way, Suite F
Medford, Or. 97504


-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Harshal Surangalikar
Sent: Friday, April 17, 2009 12:10 PM
To: [email protected]
Subject: [mems-talk] Looking for vendors/services for HDP-CVD of
SiliconNitride


Hello,

I am looking for services/vendors in the area of "high density plasma"- CVD
(HDP-CVD) of Silicon Nitride films.

The motivation to go for HDP-CVD is to get higher wet etch resistance
(BOE/Conc. HF) than that provided by the PECVD films. If any info/references
are available on improving wet etch resistance of PECVD films, that will be
very helpful as well.

Thank for the time and best regards,
Harshal Surangalikar.

Sr. MEMS Process Engineer
Fortemedia
Cupertino, CA

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation